# SeAH Superalloy Technologies to build $110M superalloy plant in Temple, Texas

SeAH Superalloy Technologies announced a $110 million investment to build a nickel-based superalloy plant in Temple, Texas, creating 100 jobs. Construction is scheduled to begin in Q3 2024, with commercial production targeted for Q1 2026.

- Type: New facility
- Announced: 2024-04-05
- Where: Temple, Texas, United States
- Value: $110.0M
- Jobs: 100
- Starts operating: Q1 2026
- Status: announced
- Capacity: 6,000 tons per year
- Products: nickel-based superalloys
- Sectors: [Steel and Metal Products](https://endata.com/sectors/steel-metal-products.md)

## Companies

- [SeAH Superalloy Technologies](https://endata.com/companies/76648.md)

## Sources

- [seahsuperalloys.com](https://www.seahsuperalloys.com/news/seah-superalloy-technologies-featured-by-temple-edc-for-temple-texas-investment), 2024-04-05: "We are proud to share that the Temple Economic Development Corporation recently published a feature highlighting our upcoming special-alloy manufacturing facility in Temple, Texas."

---
Data from Endata (https://endata.com/). Announcements are summarized from public sources and may be incomplete; check the linked originals.